ASTM A403 / A403M Grade WP316L

Chemical Properties

CarbonB ManganeseB PhosphorusB SulfurB SiliconB Nickel Chromium Molybdenum
Note B: Maximum, unless otherwise indicated.
Note E: For small diameter or thin walls, or both, where many drawing passes are required, a carbon maximum of 0.040 % is necessary in grades TP304L and TP316L. Small outside diameter tubes are defined as those less than 0.500 in. [12.7 mm] in outside diameter and light wall tubes as those less than 0.049 in. [1.24 mm] in average wall thickness.
Note F: On pierced tubing, the nickel may be 11.0–16.0 %.

Mechanical Properties

Tensile strength, min ksi [MPa] Yield strength, min, ksi [MPa] (0.2 % offset) Elongation
Standard round specimen,
min % in 4 D
Longitudinal Transverse