Chemical Properties

Copper Other
Note D: Oxygen in C10200 shall be 10 ppm max.

Mechanical Properties

Standard Former Tensile Strength, min,
ksiA
Yield Strength, min,
ksiA
Elongation in 2 in., min %
Note A: ksi = 1000 psi.