ASTM A511 / A511M Grade MT 304L

Chemical Properties

Carbon Manganese Phosphorus Sulfur Silicon Nickel Chromium
Note A: For small diameter or thin wall tubing or both, where many drawing passes are required, a maximum of 0.040 % carbon is necessary in grades MT-304L and MT-316L. Small outside diameter tubes are defined as those under a 0.500 in. [12.7 mm] outside diameter and light-wall tubes as those under a 0.049 in. [1.2 mm] average wall thickness (0.044 in. [1.1 mm] min wall thickness).

Mechanical Properties

Tensile Strength, min, ksi [MPa] Yield Strength, min, ksi [MPa] Elongation in 2 in. min, %

Products