ASTM B408 UNS N08810

Chemical Properties

Elements Composition, %
Note A: Iron shall be determined arithmetically by difference.
Note B: Alloy UNS N08811: Al + Ti, 0.85–1.20.

Mechanical Properties

Condition Tensile Strength min,
psi (Mpa)
Yield Strength (0.2 % offset) min, psi(Mpa) Elongation in 2 in. or 50 mm
(or 4D), min, %
Note B: Forging quality is furnished to chemical requirements and surface inspection only. No tensile properties are required.