ASTM A276 / A276M UNS S41040
ASTM A276 UNS S41040 is a material grade specification for
cold-finished or hot-finished bars in S41040 stainless steel,
available in form of rounds, square, hexagons and other hot rolled
extruded shapes. Ferrobend uses S41040 bar stock to ASTM A276
specifications for manufacturing stainless steel S41040 bolts, nuts,
screws, studs, threaded rods, other fasteners and bar stock
components for general engineering purposes.
ASTM A276 specification covers requirements such as chemical
composition, mechanical properties, heat treatment and other
supplementary requirements for S41040 stainless steel round bars,
square bars, hexagon bars and other extruded shapes.
Chemical Composition
Identification Symbol |
UNS Number |
Elements |
Composition % |
XM - 30
|
S41040 |
Carbon |
0.18 max |
Manganese |
1.00 max |
Phosphorus |
0.040 max |
Sulfur |
0.030 max |
Silicon |
1.00 max |
Chromium |
11.00 - 13.00 |
Columbium |
0.05 - 0.30 |
Mechanical Properties
Property |
Value |
Condition |
T |
Finish |
Hot-Finished |
Cold Finished |
Tensile Strength, min, ksi [MPa] |
125 [860] |
125 [860] |
Yield Strength, min, ksi [MPa] |
100 [690] |
100 [690] |
Elongation in 2 in. [50mm] or 4D, min, % |
13 |
12 |
Reduction or Area, min, % |
45 |
35 |
Brinell Hardness Number, HBW |
302 |
-- |
Mechanical Properties
Property |
Value |
Condition |
A |
Finish |
Hot-Finished |
Cold Finished |
Tensile Strength, min, ksi [MPa] |
70 [480] |
70 [480] |
Yield Strength, min, ksi [MPa] |
40 [275] |
40 [275] |
Elongation in 2 in. [50mm] or 4D, min, % |
13 |
12 |
Reduction or Area, min, % |
45 |
35 |
Brinell Hardness Number, HBW |
235 |
-- |