ASTM A276 UNS S31727 is a material grade specification for cold-finished or hot-finished bars in S31727 stainless steel, available in form of rounds, square, hexagons and other hot rolled extruded shapes. Ferrobend uses S31727 bar stock to ASTM A276 specifications for manufacturing stainless steel S31727 bolts, nuts, screws, studs, threaded rods, other fasteners and bar stock components for general engineering purposes.
ASTM A276 specification covers requirements such as chemical composition, mechanical properties, heat treatment and other supplementary requirements for S31727 stainless steel round bars, square bars, hexagon bars and other extruded shapes.
Identification Symbol | UNS Number | Elements | Composition % |
---|---|---|---|
... | S31727 | Carbon | 0.030 max |
Manganese | 1.00 max | ||
Phosphorus | 0.030 max | ||
Sulfur | 0.030 max | ||
Silicon | 1.00 max | ||
Chromium | 17.5 - 19.00 | ||
Nickel | 14.5 - 16.5 | ||
Molybdenum | 3.8 - 4.5 | ||
Nitrogen | 0.15 - 0.21 | ||
Copper | 2.8 - 4.0 |
Property | Value |
---|---|
Finish | Hot-Finished & Cold Finished |
Tensile Strength, min, ksi [MPa] | 80 [550] |
Yield Strength, min, ksi [MPa] | 36 [245] |
Elongation in 2 in. [50mm] or 4D, min, % | 35 |
Reduction or Area, min, % | -- |
Brinell Hardness Number, HBW | 217 |