ASTM A276 / A276M UNS S31254

ASTM A276 UNS S31254 is a material grade specification for cold-finished or hot-finished bars in S31254 stainless steel, available in form of rounds, square, hexagons and other hot rolled extruded shapes. Ferrobend uses S31254 bar stock to ASTM A276 specifications for manufacturing stainless steel S31254 bolts, nuts, screws, studs, threaded rods, other fasteners and bar stock components for general engineering purposes.

ASTM A276 specification covers requirements such as chemical composition, mechanical properties, heat treatment and other supplementary requirements for S31254 stainless steel round bars, square bars, hexagon bars and other extruded shapes.

Chemical Composition

Identification Symbol UNS Number Elements Composition %
254-smo S31254 Carbon 0.020 max
Manganese 1.00 max
Phosphorus 0.030 max
Sulfur 0.010 max
Silicon 0.80 max
Chromium 19.5 - 20.5
Nickel 17.5 - 18.5
Molybdenum 6.00 - 6.5
Nitrogen 0.18 - 0.25
Copper 0.50 - 1.00

Mechanical Properties

Property Value
Finish Hot-Finished & Cold Finished
Tensile Strength, min, ksi [MPa] 95 [650]
Yield Strength, min, ksi [MPa] 44 [300]
Elongation in 2 in. [50mm] or 4D, min, % 35
Reduction or Area, min, % 50
Brinell Hardness Number, HBW --